A shallow crater on the face of a new clay roof tile can prompt two different questions at delivery. Will the tile still do its job, and will the exposed face look acceptable alongside the approved sample? Put both questions to the supplier. A distant photograph of a stack is unlikely to settle either.
Show what came away
Sandtoft describes a manufacturing-related feature called a lime blow. A small lime inclusion just below the surface expands after exposure to moisture and dislodges the thin layer of clay above it. The producer explains that this particular expansion ends after moisture uptake. A pit in one piece is therefore a poor basis for predicting that the entire batch will keep shedding clay. Equally, the explanation cannot identify every crater from a photograph.
Use a loose tile available for inspection. Photograph the pit beside a scale, the full face showing its location, and the rear of the same piece. Record whether the recess lies on the exposed face, along a mating edge or near a fixing. Note separately any crack visible on both faces or a break at the edge. Keep the pack label and the piece together until the supplier has reviewed them. If recording frequency, state how many pieces were examined and how they were chosen.
Give each reviewer a question they can answer
Ask the producer what the observed feature means for this product and whether it recommends setting the affected pieces aside. Ask the person responsible for appearance to view the piece against the agreed reference in its intended orientation. A technical response about durability cannot settle the owner's choice of finish. Record both decisions before the material is mixed into other packs.
A line confined to a glazed finish calls for different observations. The Guild’s guide to surface lines on glazed tile describes that record.